New superalloy could cut carbon emissions from power plants

Sandia National Laboratories technologist Levi Van Bastian works to print material on the Laser Engineered Net Shaping machine, which allows scientists to 3D print new superalloys.
Credit: Craig Fritz, Sandia National Laboratories

Researchers repurpose 3D printing to discover high-performance material.

As the world looks for ways to cut greenhouse gas emissions, researchers from Sandia National Laboratories have shown that a new 3D-printed superalloy could help power plants generate more electricity while producing less carbon.

Sandia scientists, collaborating with researchers at Ames National Laboratory, Iowa State University and Bruker Corp., used a 3D printer to create a high-performance metal alloy, or superalloy, with an unusual composition that makes it stronger and lighter than state-of-the-art materials currently used in gas turbine machinery. The findings could have broad impacts across the energy sector as well as the aerospace and automotive industries, and hints at a new class of similar alloys waiting to be discovered.

“We’re showing that this material can access previously unobtainable combinations of high strength, low weight and high-temperature resiliency,” Sandia scientist Andrew Kustas said. “We think part of the reason we achieved this is because of the additive manufacturing approach.”

The team published their findings in the journal Applied Materials Today.

Material withstands high heat, essential for power plant turbines

About 80% of electricity in the U.S. comes from fossil fuel or nuclear power plants, according to the U.S. Energy Information Administration. Both types of facilities rely on heat to turn turbines that generate electricity. Power plant efficiency is limited by how hot metal turbine parts can get. If turbines can operate at higher temperatures, “then more energy can be converted to electricity while reducing the amount of waste heat released to the environment,” said Sal Rodriguez, a Sandia nuclear engineer who did not participate in the research.

Sandia’s experiments showed that the new superalloy — 42% aluminum, 25% titanium, 13% niobium, 8% zirconium, 8% molybdenum and 4% tantalum — was stronger at 800 degrees Celsius (1,472 degrees Fahrenheit) than many other high-performance alloys, including those currently used in turbine parts, and still stronger when it was brought back down to room temperature.

“This is therefore a win-win for more economical energy and for the environment,” Rodriguez said.

Energy is not the only industry that could benefit from the findings. Aerospace researchers seek out lightweight materials that stay strong in high heat. Additionally, Ames Lab scientist Nic Argibay said Ames and Sandia are partnering with industry to explore how alloys like this could be used in the automotive industry.

“Electronic structure theory led by Ames Lab was able to provide an understanding of the atomic origins of these useful properties, and we are now in the process of optimizing this new class of alloys to address manufacturing and scalability challenges,” Argibay said.

The Department of Energy and Sandia’s Laboratory Directed Research and Development program funded the research.

Discovery highlights changes in materials science

Additive manufacturing, also called 3D printing, is known as a versatile and energy-efficient manufacturing method. A common printing technique uses a high-power laser to flash-melt a material, usually a plastic or a metal. The printer then deposits that material in layers, building an object as the molten material rapidly cools and solidifies.

But this new research demonstrates how the technology also can be repurposed as a fast, efficient way to craft new materials. Sandia team members used a 3D printer to quickly melt together powdered metals and then immediately print a sample of it.

Sandia’s creation also represents a fundamental shift in alloy development because no single metal makes up more than half the material. By comparison, steel is about 98% iron combined with carbon, among other elements.

“Iron and a pinch of carbon changed the world,” Kustas said. “We have a lot of examples of where we have combined two or three elements to make a useful engineering alloy. Now, we’re starting to go into four or five or beyond within a single material. And that’s when it really starts to get interesting and challenging from materials science and metallurgical perspectives.”

Scalability, cost are challenges to overcome

Moving forward, the team is interested in exploring whether advanced computer modeling techniques could help researchers discover more members of what could be a new class of high-performance, additive manufacturing-forward superalloys.

“These are extremely complex mixtures,” said Sandia scientist Michael Chandross, an expert in atomic-scale computer modeling who was not directly involved in the study. “All these metals interact at the microscopic — even the atomic — level, and it’s those interactions that really determine how strong a metal is, how malleable it is, what its melting point will be and so forth. Our model takes a lot of the guesswork out of metallurgy because it can calculate all that and enable us to predict the performance of a new material before we fabricate it.”

Kustas said there are challenges ahead. For one, it could be difficult to produce the new superalloy in large volumes without microscopic cracks, which is a general challenge in additive manufacturing. He also said the materials that go into the alloy are expensive. So, the alloy might not be appropriate in consumer goods for which keeping cost down is a primary concern.

“With all those caveats, if this is scalable and we can make a bulk part out of this, it’s a game changer,” Kustas said.

Sandia National Laboratories is a multimission laboratory operated by National Technology and Engineering Solutions of Sandia LLC, a wholly owned subsidiary of Honeywell International Inc., for the U.S. Department of Energy’s National Nuclear Security Administration. Sandia Labs has major research and development responsibilities in nuclear deterrence, global security, defense, energy technologies and economic competitiveness, with main facilities in Albuquerque, New Mexico, and Livermore, California.

Journal: Applied Materials Today
DOI: 10.1016/j.apmt.2022.101669
Article Title: Applied Materials Today 29 (2022) 101669 Available online 17 November 2022 2352-9407/© 2022 The Authors. Published by Elsevier Ltd. This is an open access article under the CC BY license (http://creativecommons.org/licenses/by/4.0/).Extreme hardness at high temperature with a lightweight additively manufactured multi-principal element superalloy
Article Publication Date: 17-Nov-2022

Media Contact

Troy Rummler
DOE/Sandia National Laboratories
trummle@sandia.gov
Office: 505-249-3632

Media Contact

Troy Rummler
DOE/Sandia National Laboratories

All latest news from the category: Materials Sciences

Materials management deals with the research, development, manufacturing and processing of raw and industrial materials. Key aspects here are biological and medical issues, which play an increasingly important role in this field.

innovations-report offers in-depth articles related to the development and application of materials and the structure and properties of new materials.

Back to home

Comments (0)

Write a comment

Newest articles

Innovative 3D printed scaffolds offer new hope for bone healing

Researchers at the Institute for Bioengineering of Catalonia have developed novel 3D printed PLA-CaP scaffolds that promote blood vessel formation, ensuring better healing and regeneration of bone tissue. Bone is…

The surprising role of gut infection in Alzheimer’s disease

ASU- and Banner Alzheimer’s Institute-led study implicates link between a common virus and the disease, which travels from the gut to the brain and may be a target for antiviral…

Molecular gardening: New enzymes discovered for protein modification pruning

How deubiquitinases USP53 and USP54 cleave long polyubiquitin chains and how the former is linked to liver disease in children. Deubiquitinases (DUBs) are enzymes used by cells to trim protein…